Description of goods
Dark gray tablet, able to refine the grain of primary aluminium and aluminium alloys.
Function
Used in the grain-refining of trans-formative aluminium alloys
Directions for use
When the temperature of liquid aluminium reaches 720~750℃,skim off the surface dross,put the flux into the melt(flame and smoke will come into being at that time) stay still for 10 minutes after adding,stir thoroughly.the recovery of titanium to reach 90% take 30-40 minutes.
Application rate
Application rate should be 0.05-0.1% of the melt
Grain refined effectively,improve the quality of casting surface |
Reducing pinstripe,overcome the middle crack ,make grains of the casting to be at the superior grade |
Material Specification:
Density |
2..7~2.8g/cm3 |
75%-80%-85%-90%-95% |
|
1. Non-sodium flux 2 Aluminum 3 Flux + aluminum |
Package
500g or 1000g /pcs, 2kgs/bag, 20kgs/carton
Storage:
To be stored in a dry warehouse
Valid date:
12 months